MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem (Bluestar Silicones) BLUESIL™ WR 68 Water Repellent Treatment
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Methyl hydrogeno polysiloxane

Applications:

  • Water repellent treatment of plaster used to produce tiles and boards.
  • Water repellent treatment of dry-sprayed substances (e.g.: extinguisher powders, various fillers).

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Kinematic Viscosity 25 cSt25 cSt
Storage Temperature -20.0 - 30.0 °C-4.00 - 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 110 °C230 °Fclosed cup
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Appearanceclear liquid
Diluentsaliphatic or aromatic hydrocarbons, esters, ketones

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 5000 Dimethylpolysiloxane Polymer
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 50 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 20 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 1000000 Dimethylpolysiloxane Polymer
Elkem (Bluestar Silicones) BLUESIL™ FB Silicone Gum

PBLUST125 / 191108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.