Steel powder processed by DMSL. This steel has very good mechanical properties, and is easily heat-treatable using a simple thermal age-hardening process to obtain excellent hardness and strength. This material is ideal for many tooling applications (DirectTool) such as tools for injection molding, die casting of light metal alloys, punching, extrusion etc., and also for high performance industrial and engineering parts, for example in aerospace and motor racing applications.EOS®, EOSINT®, and DMLS® are registered trademarks of EOS GmbH. Information provided by Axis Prototyping. |
US classification 18% Ni Maraging 300, European 1.2709 and German X3NiCoMoTi 18-9-5 |
 Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS. Axis Proto Inc. Innovative leaders in producing high quality Rapid Prototyping and Rapid Manufacturing solutions using all major 3D printing systems including Stereolithography technology. Free online quotes at www.axisproto.comClick here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |