MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled

Material Notes: Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.

Applications:

  • Firearms
  • Automotive
  • Household appliances

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Filler Content 10 %10 %ASTM D2584
 10.0 %10.0 %TPG WI
Water Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage  0.0030 cm/cm
@Thickness 1.59 mm
0.0030 in/in
@Thickness 0.0625 in
ASTM D955
 0.00300 cm/cm
@Thickness 3.17 mm
0.00300 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 3.00 - 10.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.00 - 10.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
 105105ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Tensile Strength 65.5 MPa9500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
 3.00 %3.00 %ASTM D638
Elongation at Yield 2.00 %2.00 %ASTM D638
Tensile Modulus 4.62 GPa670 ksiASTM D638
 4.62 GPa670 ksiASTM D638
Flexural Strength 102 MPa14800 psiASTM D790
 102 MPa14800 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiTangent; ASTM D790
 4.14 GPa600 ksitangent; ASTM D790
Compressive Strength 82.7 MPa12000 psiASTM D695
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inAt 73°F; ASTM D256
 0.641 J/cm1.20 ft-lb/inASTM D256
Izod Impact, Unnotched 2.99 J/cm5.60 ft-lb/inAt 73°F; ASTM D256
Gardner Impact 0.678 J
@Thickness 12.7 mm
0.500 ft-lb
@Thickness 0.500 in
tup; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.0
@Frequency 10000 Hz
3.0
@Frequency 10000 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm450 kV/inASTM D149
Dissipation Factor 0.0080
@Frequency 10000 Hz
0.0080
@Frequency 10000 Hz
ASTM D150
Arc Resistance 80 sec80 secDry; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C
@Temperature 20.0 °C
12.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 60.0 °C140 °FContinuous use; UL 746B
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FASTM D648
 98.9 °C210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.8 °C208 °FASTM D648
 97.8 °C208 °FASTM D648
Flammability, UL94 HBHBClass 1/16
Oxygen Index <= 27 %<= 27 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 216 °C400 - 420 °F
Middle Barrel Temperature 210 - 221 °C410 - 430 °F
Front Barrel Temperature 221 - 232 °C430 - 450 °F
Nozzle Temperature 227 - 232 °C440 - 450 °F
Melt Temperature 218 - 271 °C425 - 520 °F
Mold Temperature 37.8 - 65.6 °C100 - 150 °F
Drying Temperature  71.0 °C
@Time 14400 sec
160 °F
@Time 4.00 hour
 82.0 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Back Pressure 0.172 - 0.517 MPa25.0 - 75.0 psi
Screw Speed 30.0 - 60.0 rpm30.0 - 60.0 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled

PPOLI035 / 56939

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.