MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total HP 401N Natural HDPE, pipe
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe relining

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D 792
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourNo failures; ASTM D1693 cond. C 100% lgepal
Melt Flow  0.080 g/10 min
@Load 2.16 kg
0.080 g/10 min
@Load 4.76 lb
ASTM D 1238
 0.34 g/10 min
@Load 5.00 kg
0.34 g/10 min
@Load 11.0 lb
ASTM D 1238
High Load Melt Index 7.0 g/10 min
@Load 21.6 kg
7.0 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 100 hour>= 100 hourASTM F 1473
Hardness, Shore D 6363ASTM D 2240
Tensile Strength, Yield >= 22.8 MPa>= 3300 psiASTM D 638 type IV
Elongation at Break >= 800 %>= 800 %ASTM D 638 type IV
Flexural Modulus 0.862 GPa125 ksiASTM D 790
Izod Impact, Notched 5.87 J/cm
@Thickness 3.17 mm
11.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Hydrostatic Design Basis 11.0 MPa
@Temperature 23.0 °C
1600 psi
@Temperature 73.4 °F
ASTM D 2837
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C258 °FASTM D3417

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 3802 B HDPE, cable, sheet, pipe, injection molding
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade
SCG Chemicals EL-Lene™ H5211PBL High Density Polyethylene Pipe Resin
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin

PFINAP120 / 38703

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.