System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
DuPont Teijin Films Melinex® 581 Polyester Film
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyester, TP
;
Polyester Film
Material Notes:
A super clear, one side C-Sub pretreated film for adhesion of hydrophilic coatings.
Approvals: UL Recognition - Product has been registered with Underwriters Laboratories
Information provided by DuPont.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Film Tensile Strength at Yield, MD
100
MPa
14500
psi
ASTM D882A
Film Elongation at Break, MD
170 %
170 %
ASTM D882A
Film Elongation at Break, TD
120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic
0.50
0.50
A-B; ASTM D1894
Film Tensile Strength at Break, MD
193
MPa
28000
psi
ASTM D882A
Film Tensile Strength at Break, TD
241
MPa
35000
psi
ASTM D882A
Thermal Properties
Metric
English
Comments
Shrinkage, MD
2.5 %
@Temperature 190 °C,
Time 300 sec
2.5 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD
1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties
Metric
English
Comments
Transmission, Visible
88 %
@Thickness 0.127 mm
88 %
@Thickness 0.00500 in
TLT; ASTM D1003
89 %
@Thickness 0.102 mm
89 %
@Thickness 0.00400 in
TLT; ASTM D1003
90 %
@Thickness 0.0635 mm
90 %
@Thickness 0.00250 in
TLT; ASTM D1003
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 542 Polyester Film
DuPont Teijin Films Melinex® 617 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 565 Polyester Film
DuPont Teijin Films Melinex® 561 Polyester Film
DuPont Teijin Films Melinex® 583 Polyester Film, 300 Gauge
PDTZ9166 / 139514
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.