MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem RA34U3 LLDPE Rotomolding Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: The resin RA34U3 is a linear low-density polyethylene, 1-butene based, with a good balance of processability, environmental stress cracking resistance, and impact strength. It contains long term UV6 stabilization and antioxidant additives. This resin is used to produce rotomolded parts for general use applications, kayaks, toys, and parts for the agricultural and automotive segments. This resin is recommended for rotational molding under conditions comparable to polyethylene resins with a similar melt index and density range. Oven Temperature Range: 220 to 350 ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ASTM-D1505
ESCR 100% Igepal® 400 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
400 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
ESCR 10% Igepal® 38 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
38 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiASTM-D638
Tensile Strength, Yield 17.0 MPa2470 psiASTM-D638
Elongation at Break >= 1000 %>= 1000 %ASTM-D638
Elongation at Yield 17 %17 %ASTM-D638
Flexural Modulus, 1% Secant 530 MPa76900 psiASTM-D790
Impact Test  49.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
36.1 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM
 131 J
@Thickness 6.34 mm,
Temperature -40.0 °C
96.6 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
ARM
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FASTM-D3418
Deflection Temperature at 0.46 MPa (66 psi) 56.0 °C133 °FASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C104 °FASTM-D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem RC35U4 LLDPE Rotomolding Polyethylene
Braskem RD34U3 LLDPE Rotomolding Polyethylene
Braskem ML3601U LLDPE Rotomolding Polyethylene
LyondellBasell Lupolen 3621 M RM Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Braskem ML4400N LLDPE Rotomolding Polyethylene

PBRAS877 / 106723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.