MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® T85 SG PC/ABS Blend  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: (PC+ABS)-Blend; Vicat/B 120 temperature = 130 °C; very good flow; suitable for DirectCoating /DirectSkinning

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62, 50% RH
Water Absorption at Saturation 0.60 %0.60 %ISO 62
Viscosity 255000 cP
@Shear Rate 1000 1/s,
Temperature 260 °C
255000 cP
@Shear Rate 1000 1/s,
Temperature 500 °F
melt viscosity; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.00 mm
0.0055 - 0.0075 in/in
@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
@Thickness 3.00 mm
0.0055 - 0.0075 in/in
@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Melt Flow  17 g/10 min
@Load 5.00 kg,
Temperature 260 °C
17 g/10 min
@Load 11.0 lb,
Temperature 500 °F
 17.25 g/10 min
@Load 5.01 kg,
Temperature 260 °C
17.25 g/10 min
@Load 10.8 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 54.0 MPa7830 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 55.0 MPa7980 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 4.9 %4.9 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.30 GPa334 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO)  40.0 kJ/m²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-U
Puncture Energy  46.0 J
@Temperature 23.0 °C
33.9 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 52.0 J
@Temperature -30.0 °C
38.4 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmIEC 60093
Surface Resistance 1.00e+17 ohm1.00e+17 ohmIEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0025
@Frequency 100 Hz
0.0025
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 V200 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 128 °C262 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °FISO 75-1,-2
Vicat Softening Point  129 °C
@Load 5.10 kg
264 °F
@Load 11.2 lb
50°C/h; ISO 306
 130 °C
@Load 5.10 kg
266 °F
@Load 11.2 lb
120°C/h; ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T85 XF Polycarbonate + ABS
Covestro Bayblend® T85 Polycarbonate + ABS
Covestro Bayblend® FR3010 HF PC/ABS Blend
Covestro Bayblend® T45 PG Polycarbonate + ABS
Covestro Bayblend® T65 HI PC/ABS Blend

PB09690 / 150822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.