MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cesium, Cs
Categories: Metal; Nonferrous Metal; Pure Element

Key Words: Caesium, Cs
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.89 g/cc0.0683 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 132.90546132.905461995
Atomic Number 5555
Thermal Neutron Cross Section 29 barns/atom29 barns/atom
X-ray Absorption Edge 0.34476 Å0.34476 ÅK
 2.17245 Å2.17245 ÅLI
 2.31268 Å2.31268 ÅLII
 2.47227 Å2.47227 ÅLIII
Electrode Potential -3.00 V-3.00 V
Electronegativity 0.790.79Pauling
Ionic Radius 1.67 Å1.67 ÅCrystal Ionic Radius for Valence +1
 
Mechanical PropertiesMetricEnglishComments
Bulk Modulus 1.57 GPa228 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000190 ohm-cm0.0000190 ohm-cm
Magnetic Susceptibility -2.20e-7-2.20e-7cgs/g
Critical Superconducting Temperature 1.50 K1.50 K~1.5 K for Cs V at >12.5 GPa pressure
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 15.78 J/g6.789 BTU/lb
Heat of Vaporization 611 J/g263 BTU/lb
CTE, linear  97.0 µm/m-°C
@Temperature 20.0 °C
53.9 µin/in-°F
@Temperature 68.0 °F
 284 µm/m-°C
@Temperature 50.0 °C
158 µin/in-°F
@Temperature 122 °F
liquid
Specific Heat Capacity 0.209 J/g-°C0.0500 BTU/lb-°F
Thermal Conductivity 36.0 W/m-K250 BTU-in/hr-ft²-°F
Melting Point 28.39 - 28.41 °C83.10 - 83.14 °F
Boiling Point 671 °C1240 °F
 
Component Elements PropertiesMetricEnglishComments
Cesium, Cs 100 %100 %
 
Descriptive Properties
CAS Number7440-46-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Gold, Au
Aluminum, Al
Americium, Am
Mercury, Hg

AMECs00 / 27

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.