MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alliance BCN-10 Bonded (Composite) Magnetic Material
Categories: Ceramic; Oxide; Metal; Electronic/Magnetic Alloy

Key Words: Magnet Magnets
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 5.60 - 6.00 g/cc0.202 - 0.217 lb/in³
 5.60 - 6.00 g/cc0.202 - 0.217 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 80 - 12080 - 120
Tensile Strength, Ultimate 37.0 MPa5370 psi
Modulus of Elasticity 0.700 - 1.00 GPa102 - 145 ksi
 28.0 GPa4060 ksi
Compressive Strength 27.0 - 33.0 MPa3920 - 4790 psi
 80.0 - 120 MPa11600 - 17400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00100 - 0.00300 ohm-cm0.00100 - 0.00300 ohm-cm
 0.0250 ohm-cm0.0250 ohm-cm
Magnetic Coercive Force, Hc 5500 Oe5500 Oe
 5500 - 6000 Oe5500 - 6000 Oe
 9100 Oe9100 OeIntrinsic
 8500 - 10000 Oe8500 - 10000 OeIntrinsic
Magnetic Remanence, Br 6900 Gauss6900 Gauss
 6800 - 7100 Gauss6800 - 7100 Gauss
Magnetic Maximum Energy Product, BH 10.5 MGOe10.5 MGOe
 10 - 11 MGOe10 - 11 MGOe
Curie Temperature <= 310 °C<= 590 °F
 300 - 470 °C572 - 878 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 30.0 µm/m-°C
@Temperature 20.0 °C
5.56 - 16.7 µin/in-°F
@Temperature 68.0 °F
Parallel DOM
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°F
Thermal Conductivity 2.00 W/m-K13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C248 °F
 <= 120 °C<= 248 °FLong term
 <= 160 °C<= 320 °FShort term
 
Descriptive Properties
Reversible Temperature Coefficients-0.11Bd. %/°C
 -0.39Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance A-6 Alnico Magnetic Material
Alliance A-5-7 Alnico Magnetic Material
Alliance A-8 Alnico Magnetic Material
Alliance S-28B Samarium Cobalt Magnetic Material
Alliance A-2S Alnico Magnetic Material

NALLIAN64 / 14889

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.