MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6, 30% glass fibers, injection molding, heat-aging stabilized, improved surface finish, improved resistance to weathering

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.9 %1.9 %50% RH; ISO 62
Water Absorption at Saturation 6.0 %6.0 %IOS 62
Linear Mold Shrinkage, Flow 0.0027 cm/cm0.0027 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0058 cm/cm0.0058 in/in60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  735 N
@Temperature -30.0 °C
165 lb (f)
@Temperature -22.0 °F
ISO 6603-2
 838 N
@Temperature 23.0 °C
188 lb (f)
@Temperature 73.4 °F
ISO 6603-2
Ball Indentation Hardness 230 MPa33400 psiISO 2093-1
Tensile Strength at Break 180 MPa26100 psi5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 10.0 GPa1450 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 270 MPa39200 psi2 mm/min; ISO 178-A
Flexural Modulus 9.30 GPa1350 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 4.0 %4.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  55.0 kJ/m²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 65.0 kJ/m²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 <= 1.00 J/cm²
@Temperature -40.0 °C
<= 4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 179 1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy  2.20 J
@Temperature -30.0 °C
1.62 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 2.60 J
@Temperature 23.0 °C
1.92 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
864 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.0080
@Frequency 100 Hz
0.0080
@Frequency 100 Hz
IEC 60250
 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V225 VSolution B; IEC 60112
 475 V475 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 221 °C430 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FISO 75-1,-2
Vicat Softening Point  210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
120°C/h; ISO 306
 210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 23 %23 %Method A; ISO 4589-2
Glow Wire Flammability Index 600 °C
@Thickness 2.00 mm
1110 °F
@Thickness 0.0787 in
IEC 60695-2-12
Shrinkage, MD 0.060 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.060 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.16 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.16 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °Finjection molding
 270 - 290 °C518 - 554 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.12 %0.030 - 0.12 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry)
Celanese Celstran® PP-GF50-0405P10/10 PP, 50% Glass Reinforced
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Conditioned)
Envalior Durethan® BKV 30 G H2.0 900051 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned

PLANW9380 / 208203

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.