MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ashley Polymers Ashlene® R3145-20G PC/PBT Alloy, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: A 20% glass reinforced alloy for high impact, increased mechanical strength, chemical resistance, and thermal properties.

Data provided by the manufacturer

Key Words: Polybutylene Terephthalate; Polycarbonate; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Linear Mold Shrinkage 0.0045 cm/cm0.0045 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 88.0 MPa12800 psiATSM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Modulus 5.20 GPa754 ksiASTM D790
Izod Impact, Notched 1.50 J/cm2.81 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 199 °C390 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C379 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled
Omni Plastics OmniCarb™ PC/PBT 400IM2 UV PC/PBT Alloy
Polykemi AB POLYlux 3809S F20 PC/PBT-Blend, Glass Fiber-Reinforced
Techmer ES Plastiblend® PC/PBT IM 1799 BK
Avient Edgetek® XT XT-500-CX00 PC+PBT

PNAC26 / 54612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.