MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Excellent ozone resistance.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification
  • Excellent ozone resistance.
  • EU and China RoHS compliant.
Applications:
  • Automotive-Air Induction System Ducts, Boots and Bellows for Steering and Suspension, Plugs, Bumpers, Grommets, Clips
Uses:
  • Appliance Components
  • Consumer Applications
  • Living Hinges
  • Automotive Applications
  • Diaphrams
  • Tubing
  • Automotive Under the Hood
  • Electrical Parts
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656in Air 302°F, 168 hr; ASTM D573
 51
@Thickness 2.00 mm,
Time 15.0 sec
51
@Thickness 0.0787 in,
Time 0.00417 hour
Across Flow; ISO 868
Tensile Strength, Yield 8.158 MPa1183 psi302°F, 168 hr; ASTM D573
 12.0 MPa1740 psiAcross Flow; ASTM D638
Elongation at Yield 22.6 %22.6 %302°F, 168 hr; ASTM D573
 31 %31 %Across Flow; ASTm D638
Tear Strength 87.1 kN/m497 pli73°C, Die C; ASTM D624
Compression Set  59 %
@Temperature 70.0 °C,
Time 79200 sec
59 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 74 %
@Temperature 125 °C,
Time 252000 sec
74 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.42.41.98 mm; ASTM D150
Dielectric Strength 30.7 kV/mm780 kV/in2.03 mm; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -27.8 °C-18.0 °FASTM D746
UL RTI, Electrical 85.0 °C185 °FUL 746
UL RTI, Mechanical with Impact 85.0 °C185 °FUL 746
Flammability, UL94  HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 193 °C380 °F
Middle Barrel Temperature 199 °C390 °F
Front Barrel Temperature 204 °C400 °F
Nozzle Temperature 210 - 241 °C410 - 465 °F
Die Temperature 216 °C420 °FExtrusion
Melt Temperature 210 °C410 °FExtrusion
 216 - 232 °C420 - 450 °FProcessing
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °FProcessing
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiProcessing
 5.00 - 20.0 MPa725 - 2900 psiExtrusion
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
ColorBlack
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
BASF Ultramid® B50 01 PA6
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer

PADVA047 / 22737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.