MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 600 Series Stainless Steel

Material Notes: Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) to increase its structure stability and corrosion resistance. Due to combined additions of chromium (20%), molybdenum (4.3%), copper (1.5%) combined with its high nickel content, the grade is recommended for most applications dealing with medium to severe corrosive solutions. UR B6 has improved stress corrosion resistance properties. UR B6 alloy is particularly used in sulphuric and phosphoric acids applications. The localized corrosion resistance of UR B6N grade is much higher than that of alloy 825. UR B6N is particularly well adapted to clad plates applications (separators).

Information provided by manufacturer.

Key Words: EN 10088 - EN 10028.7 X1 Ni Cr Mo Cu 25.20.5 - 1.4539, AFNOR Z2 NCDU 25.20 (AZ), DIN W. Nr 1.4539, ASTM B 625 - UNS N08904
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160 - 210160 - 210Typical, V10
Tensile Strength, Ultimate >= 550 MPa>= 79800 psiMinimum Guaranteed
Tensile Strength, Yield  >= 245 MPa
@Strain 0.2 %
>= 35500 psi
@Strain 0.2 %
 >= 275 MPa
@Strain 1 %
>= 39900 psi
@Strain 1 %
Elongation at Break >= 40 %>= 40 %
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.3330.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
10900 ksi
@Temperature 68.0 °F
Charpy Impact >= 100 J
@Temperature -196 °C
>= 73.8 ft-lb
@Temperature -321 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm
@Temperature 20.0 °C
0.0000800 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.33 µin/in-°F
@Temperature 68.0 - 212 °F
 16.0 µm/m-°C
@Temperature 20.0 - 300 °C
8.89 µin/in-°F
@Temperature 68.0 - 572 °F
 17.0 µm/m-°C
@Temperature 20.0 - 500 °C
9.44 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
0.120 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K
@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Chromium, Cr 20 %20 %
Copper, Cu 1.5 %1.5 %
Iron, Fe 49.18 %49.18 %As remainder
Molybdenum, Mo 4.3 %4.3 %
Nickel, Ni 25 %25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 904L High Performance Austenitic Stainless Steel
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36
Special Metals INCONEL® Alloy X-750

NINDUST40 / 17578

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.