MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Uniplex FRP-64 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex FRP-64 is a solid flame retardant with a high chemical resistance combined with an excellent light stability.

Chemical name: Poly (2,6-Dibromophenylene oxide)

CAS - No: 69882-11-7

Applications: Based on its high bromine content Uniplex FRP-64 imparts efficient flame retardance to a number of thermoplastics. It is used as flame retardant in unfilled and reinforced thermoplastic polyesters (PET and PBT) and polyamides (PA 6 and PA 66). It is especially recommended for applications where high chemical resistance and minimal thermal discoloration is required such as in E&E applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 210 - 240 °C410 - 464 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 64.0 %64.0 %
Iron, Fe <= 0.00020 %<= 0.00020 %<2 ppm
 
Descriptive Properties
Content<0.1%Sodium bromide
 <0.15%Tribromophenol
 <1.75%Sulfonamide
Specifications<1.0%Loss of drying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oceanchem Group Melamine Polyphosphate (MPP)
Arkema LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
Chengdu Polyster RPM540B Flame Retardant Masterbatch
Lanxess STABAXOL® KE 9193 Masterbatch Antihydrolysis agent
M Chemical GUARD DOG™ UV1577 Light Absorber, Triazene Derivative

PLANY9120 / 209511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.