MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane Solution  (discontinued **)
Categories: Fluid; Polymer

Material Notes: NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and dehumidification applications such as water management and breathable fabrics. They have a high resistance to chlorine, making water treatment a target market.

This data sheet is for solution, but MD9150 is also available as a cast membrane.

Information provided by Kraton®.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.770 - 0.800 g/cc
Solids Content 10 - 12 %
Volatiles 87 - 91 %VOCs
Viscosity 500 - 3000 cP
@Shear Rate 1.00e+10 1/s,
Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point -4.00 °FPMCC
 
Descriptive Properties
Ion Exchange Capacity1.5 meq/g
SolventCyclohexane - Heptane

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary Evoprene™ HP 3704 High Performance Thermoplastic Elastomer
AlphaGary Evoprene™ HP 3702 High Performance Thermoplastic Elastomer
Kraton® NEXAR™ MD9200 Polymer Barrier Membrane
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane
Kraton® Kraton® D-2103 Styrene-based Biomedical Elastomer

PKRA9932 / 133510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.