MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 30% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.57 g/cc0.0434 - 0.0567 lb/in³Average value: 1.28 g/cc Grade Count:59
Filler Content 30.0 %30.0 %Average value: 30.0 % Grade Count:12
Water Absorption 0.400 - 6.50 %0.400 - 6.50 %Average value: 1.71 % Grade Count:13
Moisture Absorption at Equilibrium 1.00 - 2.30 %1.00 - 2.30 %Average value: 1.73 % Grade Count:19
Water Absorption at Saturation 4.00 - 7.00 %4.00 - 7.00 %Average value: 5.26 % Grade Count:8
Additive Loading 25.0 - 30.0 %25.0 - 30.0 %Average value: 28.3 % Grade Count:3
Linear Mold Shrinkage 0.000200 - 0.0150 cm/cm0.000200 - 0.0150 in/inAverage value: 0.00239 cm/cm Grade Count:40
 0.00200 - 0.00200 cm/cm
@Temperature 80.0 - 80.0 °C
0.00200 - 0.00200 in/in
@Temperature 176 - 176 °F
Average value: 0.00200 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00200 - 0.0100 cm/cm0.00200 - 0.0100 in/inAverage value: 0.00553 cm/cm Grade Count:22
 0.00400 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
0.00400 - 0.00400 in/in
@Temperature 176 - 176 °F
Average value: 0.00400 cm/cm Grade Count:2
Melt Flow 1.00 - 5.00 g/10 min1.00 - 5.00 g/10 minAverage value: 3.00 g/10 min Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 97.0 - 12097.0 - 120Average value: 116 Grade Count:6
Tensile Strength, Ultimate 137 - 350 MPa19900 - 50800 psiAverage value: 227 MPa Grade Count:59
 65.0 - 260 MPa
@Temperature -40.0 - 150 °C
9430 - 37700 psi
@Temperature -40.0 - 302 °F
Average value: 130 MPa Grade Count:4
Elongation at Break 1.00 - 12.3 %1.00 - 12.3 %Average value: 2.40 % Grade Count:59
 2.30 - 5.00 %
@Temperature 60.0 - 150 °C
2.30 - 5.00 %
@Temperature 140 - 302 °F
Average value: 3.58 % Grade Count:3
Modulus of Elasticity 14.0 - 33.1 GPa2030 - 4800 ksiAverage value: 21.0 GPa Grade Count:52
 4.90 - 21.5 GPa
@Temperature 60.0 - 150 °C
711 - 3120 ksi
@Temperature 140 - 302 °F
Average value: 11.4 GPa Grade Count:3
Flexural Yield Strength 215 - 456 MPa31200 - 66100 psiAverage value: 343 MPa Grade Count:36
 140 - 337 MPa
@Temperature -40.0 - 80.0 °C
20300 - 48900 psi
@Temperature -40.0 - 176 °F
Average value: 252 MPa Grade Count:1
Flexural Modulus 10.0 - 29.0 GPa1450 - 4200 ksiAverage value: 18.3 GPa Grade Count:37
 7.20 - 19.0 GPa
@Temperature -40.0 - 80.0 °C
1040 - 2760 ksi
@Temperature -40.0 - 176 °F
Average value: 13.4 GPa Grade Count:1
Flexural Strain at Break 2.50 - 3.10 %2.50 - 3.10 %Average value: 2.90 % Grade Count:3
Izod Impact, Notched 0.534 - 2.40 J/cm1.00 - 4.50 ft-lb/inAverage value: 1.22 J/cm Grade Count:20
 0.720 - 0.800 J/cm
@Temperature -40.0 - -40.0 °C
1.35 - 1.50 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.760 J/cm Grade Count:1
Izod Impact, Unnotched 6.41 - 10.7 J/cm12.0 - 20.0 ft-lb/inAverage value: 8.27 J/cm Grade Count:13
Izod Impact, Notched (ISO) 7.00 - 24.0 kJ/m²3.33 - 11.4 ft-lb/in²Average value: 10.6 kJ/m² Grade Count:12
 6.00 - 16.0 kJ/m²
@Temperature -30.0 - -30.0 °C
2.86 - 7.61 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 10.0 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) 43.0 - 80.0 kJ/m²20.5 - 38.1 ft-lb/in²Average value: 58.4 kJ/m² Grade Count:7
 45.0 - 75.0 kJ/m²
@Temperature -30.0 - -30.0 °C
21.4 - 35.7 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 64.0 kJ/m² Grade Count:4
Charpy Impact Unnotched 2.30 - 11.0 J/cm²10.9 - 52.4 ft-lb/in²Average value: 5.93 J/cm² Grade Count:25
 2.10 - 8.50 J/cm²
@Temperature -40.0 - -20.0 °C
9.99 - 40.5 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 4.83 J/cm² Grade Count:9
Charpy Impact, Notched 0.500 - 2.20 J/cm²2.38 - 10.5 ft-lb/in²Average value: 1.03 J/cm² Grade Count:25
 0.500 - 1.00 J/cm²
@Temperature -40.0 - -20.0 °C
2.38 - 4.76 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.665 J/cm² Grade Count:8
Dart Drop, Total Energy  6.19 - 12.2 J
@Temperature -20.0 - -20.0 °C
4.57 - 9.00 ft-lb
@Temperature -4.00 - -4.00 °F
Average value: 9.19 J Grade Count:1
 6.19 - 12.2 J
@Thickness 3.18 - 3.18 mm
4.57 - 9.00 ft-lb
@Thickness 0.125 - 0.125 in
Average value: 9.19 J Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00500 - 200000 ohm-cm0.00500 - 200000 ohm-cmAverage value: 9210 ohm-cm Grade Count:27
Surface Resistance 10.0 ohm - 1e+0510.0 ohm - 1e+05Average value: 4510 ohm Grade Count:23
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 - 25.0 µm/m-°C3.33 - 13.9 µin/in-°FAverage value: 17.1 µm/m-°C Grade Count:7
Melting Point 221 - 265 °C430 - 509 °FAverage value: 258 °C Grade Count:25
Maximum Service Temperature, Air 100 - 250 °C212 - 482 °FAverage value: 146 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 240 - 260 °C464 - 500 °FAverage value: 255 °C Grade Count:23
Deflection Temperature at 1.8 MPa (264 psi) 230 - 270 °C446 - 518 °FAverage value: 250 °C Grade Count:44
Vicat Softening Point 230 - 255 °C446 - 491 °FAverage value: 247 °C Grade Count:10
Glass Transition Temp, Tg 5.00 - 72.0 °C41.0 - 162 °FAverage value: 38.5 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:30
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 310 °C518 - 590 °FAverage value: 286 °C Grade Count:8
Nozzle Temperature 270 - 320 °C518 - 608 °FAverage value: 283 °C Grade Count:9
Melt Temperature 260 - 320 °C500 - 608 °FAverage value: 285 °C Grade Count:41
Mold Temperature 60.0 - 140 °C140 - 284 °FAverage value: 89.7 °C Grade Count:45
Drying Temperature 79.4 - 120 °C175 - 248 °FAverage value: 90.3 °C Grade Count:38
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.157 % Grade Count:13
Dew Point -28.9 - -17.8 °C-20.0 - 0.000 °FAverage value: -19.6 °C Grade Count:6
Injection Pressure 30.0 - 124 MPa4350 - 18000 psiAverage value: 88.2 MPa Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Carbon Fiber Filled

O2523 / 78022

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.