MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.20 - 1.57 g/ccAverage value: 1.28 g/cc Grade Count:59
Filler Content 30.0 %Average value: 30.0 % Grade Count:12
Water Absorption 0.400 - 6.50 %Average value: 1.71 % Grade Count:13
Moisture Absorption at Equilibrium 1.00 - 2.30 %Average value: 1.73 % Grade Count:19
Water Absorption at Saturation 4.00 - 7.00 %Average value: 5.26 % Grade Count:8
Additive Loading 25.0 - 30.0 %Average value: 28.3 % Grade Count:3
Linear Mold Shrinkage 0.000200 - 0.0150 cm/cmAverage value: 0.00239 cm/cm Grade Count:40
 0.00200 - 0.00200 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00200 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00200 - 0.0100 cm/cmAverage value: 0.00553 cm/cm Grade Count:22
 0.00400 - 0.00400 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00400 cm/cm Grade Count:2
Melt Flow 1.00 - 5.00 g/10 minAverage value: 3.00 g/10 min Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 97.0 - 120Average value: 116 Grade Count:6
Tensile Strength, Ultimate 137 - 350 MPaAverage value: 227 MPa Grade Count:59
 65.0 - 260 MPa
@Temperature -40.0 - 150 °C
Average value: 130 MPa Grade Count:4
Elongation at Break 1.00 - 12.3 %Average value: 2.40 % Grade Count:59
 2.30 - 5.00 %
@Temperature 60.0 - 150 °C
Average value: 3.58 % Grade Count:3
Modulus of Elasticity 14.0 - 33.1 GPaAverage value: 21.0 GPa Grade Count:52
 4.90 - 21.5 GPa
@Temperature 60.0 - 150 °C
Average value: 11.4 GPa Grade Count:3
Flexural Yield Strength 215 - 456 MPaAverage value: 343 MPa Grade Count:36
 140 - 337 MPa
@Temperature -40.0 - 80.0 °C
Average value: 252 MPa Grade Count:1
Flexural Modulus 10.0 - 29.0 GPaAverage value: 18.3 GPa Grade Count:37
 7.20 - 19.0 GPa
@Temperature -40.0 - 80.0 °C
Average value: 13.4 GPa Grade Count:1
Flexural Strain at Break 2.50 - 3.10 %Average value: 2.90 % Grade Count:3
Izod Impact, Notched 0.534 - 2.40 J/cmAverage value: 1.22 J/cm Grade Count:20
 0.720 - 0.800 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 0.760 J/cm Grade Count:1
Izod Impact, Unnotched 6.41 - 10.7 J/cmAverage value: 8.27 J/cm Grade Count:13
Izod Impact, Notched (ISO) 7.00 - 24.0 kJ/m²Average value: 10.6 kJ/m² Grade Count:12
 6.00 - 16.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 10.0 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) 43.0 - 80.0 kJ/m²Average value: 58.4 kJ/m² Grade Count:7
 45.0 - 75.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 64.0 kJ/m² Grade Count:4
Charpy Impact Unnotched 2.30 - 11.0 J/cm²Average value: 5.93 J/cm² Grade Count:25
 2.10 - 8.50 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 4.83 J/cm² Grade Count:9
Charpy Impact, Notched 0.500 - 2.20 J/cm²Average value: 1.03 J/cm² Grade Count:25
 0.500 - 1.00 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.665 J/cm² Grade Count:8
Dart Drop, Total Energy 6.19 - 12.2 J
@Temperature -20.0 - -20.0 °C
Average value: 9.19 J Grade Count:1
 6.19 - 12.2 J
@Thickness 3.18 - 3.18 mm
Average value: 9.19 J Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00500 - 200000 ohm-cmAverage value: 9210 ohm-cm Grade Count:27
Surface Resistance 10.0 ohm - 1e+05Average value: 4510 ohm Grade Count:23
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 - 25.0 µm/m-°CAverage value: 17.1 µm/m-°C Grade Count:7
Melting Point 221 - 265 °CAverage value: 258 °C Grade Count:25
Maximum Service Temperature, Air 100 - 250 °CAverage value: 146 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 240 - 260 °CAverage value: 255 °C Grade Count:23
Deflection Temperature at 1.8 MPa (264 psi) 230 - 270 °CAverage value: 250 °C Grade Count:44
Vicat Softening Point 230 - 255 °CAverage value: 247 °C Grade Count:10
Glass Transition Temp, Tg 5.00 - 72.0 °CAverage value: 38.5 °C Grade Count:3
Flammability, UL94 HB - V-0Grade Count:30
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 310 °CAverage value: 286 °C Grade Count:8
Nozzle Temperature 270 - 320 °CAverage value: 283 °C Grade Count:9
Melt Temperature 260 - 320 °CAverage value: 285 °C Grade Count:41
Mold Temperature 60.0 - 140 °CAverage value: 89.7 °C Grade Count:45
Drying Temperature 79.4 - 120 °CAverage value: 90.3 °C Grade Count:38
Moisture Content 0.0300 - 0.200 %Average value: 0.157 % Grade Count:13
Dew Point -28.9 - -17.8 °CAverage value: -19.6 °C Grade Count:6
Injection Pressure 30.0 - 124 MPaAverage value: 88.2 MPa Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Carbon Fiber Filled

O2523 / 78022

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.