MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Primacor® 5990I Ethylene Acrylic Acid (EAA)
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: PRIMACOR® 5990I is an ethylene acrylic acid copolymer (20 wt % comonomer) for specialty hot melt adhesive applications. Its outstanding properties include toughness and adhesion to a wide variety of difficult to bond substrates, such as metals, nylon, glass and urethanes. When used unmodified for food packaging applications, this resin complies with the U.S. Food, Drug and Cosmetic Act as amended under Food Additive Regulation 21 CFR 177.1310(c). The regulation should be consulted for complete details.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/cc
Melt Flow 1300 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 42
Tensile Strength, Ultimate 6.20 MPa
Elongation at Break 350 %
Modulus of Elasticity 0.0221 GPaMolded Sample 2% Secant Modulus
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 40.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Primacor® 5980I Ethylene Acrylic Acid (EAA)
Dow Primacor® 5986 Ethylene acrylic acid copolymer
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3440 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3150 Ethylene Acrylic Acid (EAA)

PDW533 / 34602

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.