MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Linear Mold Shrinkage, Flow 0.0035 - 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.0095 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa
@Temperature 150 °C
 65.0 MPa
@Temperature 120 °C
 80.0 MPa
@Temperature 90.0 °C
 105 MPa
@Temperature 60.0 °C
 155 MPa
@Temperature 23.0 °C
Elongation at Break 3.0 %
@Temperature 23.0 °C
 5.5 %
@Temperature 60.0 °C
 6.0 %
@Temperature 90.0 °C
 6.5 %
@Temperature 120 °C
 7.0 %
@Temperature 150 °C
Elongation at Yield 3.0 %
@Temperature 23.0 °C
 5.0 %
@Temperature 60.0 °C
 5.8 %
@Temperature 90.0 °C
 6.0 %
@Temperature 120 °C
 6.0 %
@Temperature 150 °C
Tensile Modulus 3200 MPa
@Temperature 150 °C
 3600 MPa
@Temperature 120 °C
 4600 MPa
@Temperature 90.0 °C
 6100 MPa
@Temperature 60.0 °C
 9300 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
 63.0 kJ/m²
@Temperature -20.0 °C
Charpy Impact, Notched 6.50 kJ/m²
@Temperature -20.0 °C
 9.50 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
Vicat Softening Point 215 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 260 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
LATI Latamid 66 PA 66
Versalis Riblene® MP 30 Low Density Polyethylene - Injection Molding
Celanese Zytel® 73G30HSL BK416 PA6-GF30
Envalior Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber

PLATH9682 / 177378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.