MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elix Polymers ELIX PC/ABS 5130 Polycarbonate/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: PC/ABS blend, injection molding grade that poses a good combination of impact, stiffness and toughness. Vicat B120 = 130ºC

Major Benefits:

  • Easy flow
  • Very high impact up to -40ºC
  • Low emission grade
  • UV stabilized grade
  • Good stability even with high humidity conditions
  • Low shrinkage
  • Good paintability
  • Thin-walled parts
Chemical composition: Thermoplastic polymer blend based on polycarbonate (PC) and acrylonitrile-butadienestyrene (ABS).

Physical form: White to slightly yellowish pellets

Information provided by Elix Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %50% RH; ISO 62
Water Absorption at Saturation 0.70 %ISO 62
Linear Mold Shrinkage, Flow 0.0065 - 0.0075 cm/cm60x60x2 mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0065 - 0.0075 cm/cm60x60x2 mm; ISO 294-4
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 28 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2270 MPa1 mm/min; ISO 527-1,-2
Flexural Modulus 2280 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) >= 30.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 30.0 kJ/m²
@Temperature -40.0 °C
ISO 180-1A
 >= 38.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 77.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 81.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 123 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 104 °CISO 75-1,-2
Vicat Softening Point 130 °C
@Load 12.2 kg
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Descriptive Properties
Burning rate<80 mm/minUS-FMVSS, ISO 3795, 150x105x1 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elix Polymers Elix™ PC/5130 PC/ABS Polymer
Elix Polymers Elix™ 114 H ABS Polymer Modifier
Elix Polymers ELIX PC/ABS 5120 Polycarbonate/ABS Alloy
Elix Polymers Elix™ Ultra HH 4115 PG ABS Polymer
Elix Polymers ELIX ABS P3H-AT Acrylonitrile Butadiene Styrene (ABS)

PELIX031 / 183346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.