MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Niobium, Nb; Unalloyed RG (UNS R04200)
Categories: Metal; Nonferrous Metal; Niobium Alloy; Refractory Metal; Pure Element

Material Notes: Reactor-grade unalloyed niobium

Key Words: UNS R04200
Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.57 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 80 - 120
Tensile Strength, Ultimate 275 - 585 MPa
Tensile Strength, Yield 207 MPa
@Strain 0.2 %
Elongation at Break 5.0 - 30 %
Modulus of Elasticity 103 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000125 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.270 J/g-°C
Thermal Conductivity 52.3 W/m-K
Melting Point 2468 °C
Boiling Point 4744 °C
 
Component Elements PropertiesOriginal ValueComments
Niobium, Nb (Columbium, Cb) 100 %impurity levels unquantified

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Niobium, Nb; High Purity
Niobium, Nb (Columbium, Cb); Annealed Sample
Niobium, Nb; Hard
Niobium, Nb; Soft
Niobium FS-85 (Nb-28Ta-10W-1Zr), Stress Relieved

MRNb53 / 100346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.