MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanthanum, La
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes:

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.166 g/cc0.2228 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 138.9055138.90551995
Atomic Number 5757
X-ray Absorption Edge 0.31842 Å0.31842 ÅK
 1.97892 Å1.97892 ÅLI
 2.1003 Å2.1003 ÅLII
 2.25792 Å2.25792 ÅLIII
Electronegativity 1.11.1Pauling
Ionic Radius 1.016 Å1.016 ÅCrystal Ionic Radius for Valence +3
 1.39 Å1.39 ÅCrystal Ionic Radius for Valence +1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 2828
Tensile Strength, Ultimate 130 MPa18900 psi
Tensile Strength, Yield 125 MPa18100 psi
Elongation at Break 7.9 %7.9 %
Tensile Modulus 36.6 GPa5310 ksi
Bulk Modulus 27.9 GPa4050 ksi
Poissons Ratio 0.280.28
Shear Modulus 14.3 GPa2070 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000798 ohm-cm0.0000798 ohm-cm
Magnetic Susceptibility 7.27e-77.27e-7cgs/g
Critical Magnetic Field Strength, Oersted 800800or alpha phase
 10961096beta phase
Critical Superconducting Temperature 9.20 K9.20 K~5.5-12.9 K from 0-21.0 GPa pressure; 4.88 for alpha phase. Value for ßLa is 6.00 K.
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 44.6 J/g19.2 BTU/lb
CTE, linear 12.1 µm/m-°C
@Temperature 20.0 °C
6.72 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.1641 J/g-°C0.03923 BTU/lb-°FGas
 0.1951 J/g-°C0.04663 BTU/lb-°FCrystal
Thermal Conductivity 14.0 W/m-K97.2 BTU-in/hr-ft²-°F
Melting Point 915 - 925 °C1680 - 1700 °F
Boiling Point 3464 °C6267 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 431 kJ/mol431 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.409
@Wavelength >=645 nm,
Temperature 867 - 918 °C
0.409
@Wavelength >=645 nm,
Temperature 1590 - 1680 °F
 
Component Elements PropertiesMetricEnglishComments
Lanthanum, La 100 %100 %
 
Descriptive Properties
CAS Number7439-91-0
SolubilitySoluble in diluted Acid

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO35 Temper flat products
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO50 Temper rod
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO70 Temper flat products
Low-silicon bronze B, UNS C65100, H00 Temper 2 mm wire

AMELa00 / 53

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.