MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUTENE CCO550BK PE Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smooth glossy surface. LUTENE CC0550BK contains 2.6wt% finely dispersed carbon black and antioxidants, both of which together give an excellent resistance to thermal and oxidative degradations.

Applications: Sheathing of telecommunication and power cable

CAS No: 1333-86-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.935 g/ccASTM D1505
Environmental Stress Crack Resistance >= 2000 hourASTM D1693
Carbon Black Loading 2.6 %ASTM D1603
Melt Flow 0.95 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48ASTM D2240
Tensile Strength at Break 14.22 MPa500mm/min; ASTM D638
 13.5 MPa
@Treatment Temp. 110 °C,
Time 1.21e+6 sec
500mm/min; ASTM D638
Elongation at Break 700 %ASTM D638
 >= 665 %
@Treatment Temp. 110 °C,
Time 1.21e+6 sec
ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 - 130 °C
Brittleness Temperature <= -76.0 °CASTM D746
 
Descriptive Properties
Stripping force4-5 kg/12.7/mm500mm/min, ASTM D903
UV Absorption Coefficient>4000ASMT D3349

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUTENE FB0300 LDPE Blown Film Grade
LG Chemical LUTENE BB0808 LDPE Blown Film Grade
LG Chemical LUTENE FB0800 LDPE Blown Film
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Film Grade

PLAY697 / 148707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.