MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel AIRKOOL® (AISI A2) Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Medium Alloy Steel; Tool Steel; Air-Hardening Steel

Material Notes: Airkool (AISI A2) is an air-hardening medium alloy tool steel which is heat treatable to HRC 60-62. It has wear resistance intermediate between the oil hardening tool steels (O1) and the high carbon chromium tool steels (D2). Because it offers a combination of good toughness along with moderate wear resistance, it has been widely used for many years in variety of cold work applications which require fairly high abrasion resistance but where the higher carbon/ high chromium steels are prone to chipping and cracking. Airkool is quite easily machined in the annealed condition and, like other air-hardening tool steels, exhibits minimal distortion on hardening, making it an excellent choice for dies of complicated design.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.86 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 197 - 241Annealed
Hardness, Rockwell C 60 - 62
Modulus of Elasticity 207 GPa
Charpy Impact 53.0 JAustenitizing Temperature- 955°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.6 µm/m-°C
@Temperature 20.0 - 260 °C
 14.0 µm/m-°C
@Temperature 20.0 - 540 °C
Thermal Conductivity 26.0 W/m-K
@Temperature 95.0 °C
Shrinkage -0.0600 %
@Temperature 540 - 620 °C
Tempered at 540-620°C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.0 %
Chromium, Cr 5.25 %
Iron, Fe 91.55 %As Remainder
Manganese, Mn 0.85 %
Molybdenum, Mo 1.1 %
Vanadium, V 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type A2 Tool Steel
Bohler-Uddeholm AISI A2 Cold Work Tool Steel
Carpenter No. 484® (Carpenter Air-Hard; AISI A2)
Crucible Steel PM M2 Tool Steel
Latrobe LSS™ A2 Tool Steel (ASTM A2)

NCRUC022 / 16015

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.