MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes:
    Features:
  • UL HB @ 1.6-3.2mm
  • Excellent balance properties
  • High stiffness
  • Good size stability
  • Good surface adhesion
  • Excellent processing properties, large parts

    Applications:
  • Injection molding
  • Automobile instrument panel
  • CD-ROM base pick-up
  • OA device and parts

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/cc
@Temperature 23.0 °C
ASTM D792
Filler Content 10 %Glass Fiber
Water Absorption 0.12 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Temperature 23.0 °C
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82ASTM D785
Tensile Strength at Break 76.0 MPa10mm/min; ASTM D638
Elongation at Break 7.0 %10mm/min; ASTM D638
Flexural Strength 119 MPa2mm/min; ASTM D790
Flexural Modulus 4350 MPa2mm/min; ASTM D790
Izod Impact, Notched 75.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 2.80 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Strength 28.0 kV/mm1.6mm; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 285 °C
Rear Barrel Temperature 240 - 260 °CStart Point: 250°C
Middle Barrel Temperature 245 - 270 °CStart Point: 255°C
Front Barrel Temperature 250 - 280 °CStart Point: 260°C
Melt Temperature 240 - 270 °CStart Point: 260°C
Mold Temperature 80.0 - 130 °CStart Point: 90°C
Drying Temperature 100 - 110 °C
@Time 14400 - 21600 sec
Pre-dry
Back Pressure 0.000 - 0.700 MPa
 
Descriptive Properties
Injection Speed60-90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled
LATI LASTILAC 11 G/20-V0 20% Glass Fiber Reinforced ABS/PC-Based Alloy
A. Schulman Diamond ABSPC 9901GF20 Injection Molding Grade, 20% Glass Filled
Covestro Bayblend® FR 3310 TV PC/ABS Blend, 15% Glass Reinforced
Covestro Bayblend® FR 3311 TV PC/ABS Blend, 15% Glass Reinforced

PKINGF078 / 104337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.