MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times while maintaining excellent properties. It exhibits high strength, rigidity and heat resistance. Surface appearance has been improved, cycle times reduced and creep resistance retained. This heat stabilizer version extends the retention of mechanical properties at elevated temperatures while maintaining excellent chemical resistance to greases, oils and hydrocarbons.

Applications: window locks, valve bodies, chair shells, door and window hardware, connectors, switch components, relay parts, terminal blocks, power tool housings, gears, chainsaws, blowers, trimmer housings and automotive housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccASTM D792
Moisture Absorption at Equilibrium 1.1 %24 Hours; ASTM D570
 1.8 %50% RH; ASTM D570
 6.4 %Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm1/8" bar
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength at Break 175 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 256 MPaASTM D790
Flexural Modulus 9380 MPaASTM D790
Izod Impact, Notched (ISO) 95.0 kJ/m²ASTM D256
Dart Drop, Total Energy 4.61 JBASF
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmASTM D257
Dielectric Strength 22.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°CASTM E831
Melting Point 220 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 208 °CASTM D648
UL RTI, Electrical 140 °C
@Thickness 1.50 mm
746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
746B
UL RTI, Mechanical without Impact 140 °C
@Thickness 1.50 mm
746B
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 295 °C
Mold Temperature 80.0 - 95.0 °C
Dry Time 2 - 4 hour
Moisture Content <= 0.10 %
 
Descriptive Properties
ColorBK 102
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY

PBASG0424 / 132057

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.