MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Description: Injection Molding, PC/ABS, Flame Retardant

Application: Electric and Electronic Housing and Components

CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength, Yield 520 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 60 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 800 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 22000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched 45.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 85.0 °C
@Thickness >=0.750 mm
 85.0 °C
@Thickness >=1.70 mm
 85.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 75.0 °C
@Thickness >=0.750 mm
 75.0 °C
@Thickness >=1.70 mm
 75.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 75.0 °C
@Thickness >=0.750 mm
 75.0 °C
@Thickness >=1.70 mm
 75.0 °C
@Thickness >=3.00 mm
Flammability, UL94 V-0
@Thickness >=0.750 mm
 V-0
@Thickness >=1.70 mm
 5VB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 270 °CInjection Molding
Middle Barrel Temperature 245 - 275 °CInjection Molding
Front Barrel Temperature 245 - 275 °CInjection Molding
Nozzle Temperature 245 - 275 °CInjection Molding
Melt Temperature 240 - 270 °CInjection Molding
Mold Temperature 50.0 - 70.0 °CInjection Molding
Drying Temperature 80.0 - 100 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Polymers Tekaloy® G70F2 G70NH, Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate

PLAY597 / 148607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.