MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C62300 (Aluminum Bronze 9%), H50 Temper, 25 mm rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability. Fabricated by bending, hot pressing, forming, and welding.

Applications: bearings, bushings, valve guides, gears, valve seats, nuts, bolts, pump rods, work gears, and cams.

Test specimen: rod - =25mm diameter.

Key Words: CDA 623, CA106, ISO CuAl8Fe3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 89
Tensile Strength, Ultimate 605 MPa
Tensile Strength, Yield 305 MPaDepending on temper
Elongation at Break 15 %in 50 mm, 15% reduction in area
Modulus of Elasticity 115 GPa
Compressive Yield Strength 52.0 ksiAt permanent set of 0.1%
 70.0 ksiAt permanent set of 1%
 120 ksiAt permanent set of 10%
 140 ksiAt permanent set of 20%
Poissons Ratio 0.328
Fatigue Strength 200 MPa
@# of Cycles 1.00e+8
Reverse Bending; Temper Not Reported
Machinability 50 %
Forgeability 75 %
Shear Modulus 44.0 GPa
Izod Impact 43.0 - 47.0 JTemper not specified
Charpy Impact 25.0 - 40.0 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.17
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.375 J/g-°C
Thermal Conductivity 54.4 W/m-K
@Temperature 20.0 °C
Melting Point 1040 - 1045 °C
Solidus 1040 °C
Liquidus 1045 °C
Annealing Point 1100 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1010 °CHot-Shortness Temperature
Annealing Temperature 600 - 650 °C
Hot-Working Temperature 700 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 8.5 - 11 %
Copper, Cu 82.2 - 89.5 %
Iron, Fe 2.0 - 4.0 %
Manganese, Mn <= 0.50 %
Other, total <= 0.50 %
Silicon, Si <= 0.25 %
Tin, Sn <= 0.60 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C62300 (Aluminum Bronze 9%)
Copper, UNS C62300 (Aluminum Bronze 9%), Annealed Rod
Copper, UNS C62300 (Aluminum Bronze 9%), Cold Finished Rod
Copper, UNS C62300 (Aluminum Bronze 9%), H50 Temper 25-50 mm rod
Aluminum Bronze, UNS C61300, H04 Temper

MC62300b2 / 11603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.