MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 9095AU Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; with special UV stabilizers; very good hydrolysis and microbial resistance; good wear resistance; low warparge; short cycle times; Application; Ear-tags

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ISO 868
Tensile Strength, Ultimate 52.7 MPa200 mm/min; DIN 53504
Tensile Stress at Strain 6.40 MPa
@Strain 10 %
200 mm/min; DIN 53504
 12.0 MPa
@Strain 50 %
200 mm/min; DIN 53504
 14.8 MPa
@Strain 100 %
200 mm/min; DIN 53504
 30.0 MPa
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 450 %200 mm/min; DIN 53504
Tensile Modulus 0.0820 GPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
 0.161 GPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
 0.790 GPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
Rebound 33 %Resilience; ISO 4662
Tear Strength 129 kN/m500 mm/min; ISO 34-1
Abrasion 18mm³. Method A; ISO 4649
Compression Set 30 %
@Temperature 23.0 °C
72 hr; ISO 815
 43 %
@Temperature 70.0 °C
24 hr; ISO 815
 31 %
@Temperature 70.0 °C,
Time 86400 sec
Method C; ISO 815-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 220 °CInjection
Mold Temperature 20.0 °CInjection
Drying Temperature 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 1350D Polyurethane
Avient Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE)
Covestro Desmopan® 3055D Polyurethane
Covestro Desmopan® 3072D Polyurethane
Covestro Desmopan® 9868DU Polyurethane

PB09812 / 92652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.