MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: RX® 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.

Information supplied by Sumitomo Bakelite North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.900 g/ccPowder; ISO 60
Density 1.81 g/ccISO 1183
Water Absorption 0.060 %ISO 62
Linear Mold Shrinkage 0.0020 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ISO 2039/2
Tensile Strength, Ultimate 70.0 MPaISO 527
Flexural Strength 120 MPaISO 178
Flexural Modulus 17.0 GPaISO 178
Compressive Strength 270 MPaISO 604
Charpy Impact Unnotched 0.570 J/cm²ISO 179
Charpy Impact, Notched 0.270 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+13 ohm-cmIEC 93
Surface Resistance 1.56e+13 ohmIEC 93
Dielectric Strength 24.9 kV/mm
@Thickness 3.00 mm
IEC 243
Arc Resistance 180 secASTM D495
Comparative Tracking Index 200 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.0 µm/m-°C
@Temperature 23.0 °C
TMA
CTE, linear, Transverse to Flow 26.8 µm/m-°C
@Temperature 20.0 °C
TMA
Thermal Conductivity 0.690 W/m-KASTM F433
Maximum Service Temperature, Air 180 °CUL Temperature Index; UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 200 °CAs Molded; ISO 75 A
 >= 282 °CPost Baked; ISO 75 A
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
 
Descriptive Properties
Available Molding GradesCompression, Transfer, Injection
ColorBlack, Green
FormGranular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Overview of materials for Phenolic; Unreinforced; Molded
Covestro Desmopan® 372 Thermoplastic Polyurethane
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Raschig Group DECAL® 5431 Phenolic

P90XR02 / 21216

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.