MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Addisil™ 482 E Healthcare Extrusion Grade Heat Cured Rubber  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.

Addisil 482 E is a member of the Addisil Addition Curing Portfolio. It is a platinum (addition/heat) curable, two-part system with a mixing ratio of A:B 1:1. This grade is suitable for extrusion and intended for application in the Healthcare industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 81
Tensile Strength 9.00 MPa
Elongation at Break 400 %
Tear Strength 30.0 kN/mDie B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %transparent; thickness unknown
 
Compliance PropertiesOriginal ValueComments
FDA YesFDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
 
Descriptive Properties
AppearanceTransparent
BfRproduct is compositionally compliantRecommendation XV Silicones; post cured (4h/200°C)
ISO10993yes7 ISO 10993 tests applicable to "wet" chemicals

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED-4080 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
Momentive Performance Materials TSE 2287U Heat Cured Rubber - High Duro Translucent
Momentive Performance Materials Silopren™ LSR 4640 Liquid Silicone Rubber - Healthcare
Momentive Performance Materials Addisil™ 1140 M Industrial Molding Heat Cured Rubber
Dow Silastic® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT

PGE8V820 / 109080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.