MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellent clarity and flexibility for low modulus applications. Its low specific gravity (density) delivers lighter weight parts. The product form is free-flowing pellets.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 g/ccASTM D792
Melt Index of Compound <= 2.0 g/10 min
@Load 2.00 kg,
Temperature 190 °C
ASTM D1238
 22.5 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6810 sec; ASTM D2240
Tensile Strength, Ultimate 7.20 MPaASTM D412
Elongation at Break 1000 %ASTM D412
100% Modulus 0.0370 GPa
@Strain 100 %
2% Secant Modulus 0.0110 GPaASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer
Dow Engage® 8842 Polyolefin Elastomer
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer
Dow Engage® 8540 Polyolefin Elastomer
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer

PDVE53 / 34114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.