System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical TR558A MABS, Injection Molding Grade
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Material Notes:
Transparency, General Purpose
Applications: Electric & Electronic Products
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.11
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0070
cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow
25
g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
113
ASTM D785
Tensile Strength, Yield
530
kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break
>= 15 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Yield
5.0 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Tensile Modulus
2350
MPa
@Thickness 3.20 mm
50 mm/min; ASTM D638
Flexural Strength
79.0
MPa
@Thickness 3.20 mm
15 mm/min; ASTM D790
Flexural Modulus
26000
kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Izod Impact, Notched
3.57
kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
3.57
kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
11.7
kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
12.8
kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
83.0
°C
@Thickness 6.40 mm
Unannealed, Edgewise; ASTM D648
Vicat Softening Point
83.0
°C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical
60.0
°C
UL 746B
UL RTI, Mechanical with Impact
60.0
°C
UL 746B
UL RTI, Mechanical without Impact
60.0
°C
UL 746B
Flammability, UL94
HB
@Thickness 1.50 mm
HB
@Thickness 3.00 mm
Optical Properties
Original Value
Comments
Haze
1.8 %
ASTM D1003
Transmission, Visible
90 %
@Thickness 3.20 mm
ASTM D1003
Processing Properties
Original Value
Comments
Rear Barrel Temperature
180
-
200
°C
Middle Barrel Temperature
190
-
210
°C
Front Barrel Temperature
200
-
220
°C
Nozzle Temperature
200
-
230
°C
Melt Temperature
200
-
230
°C
Mold Temperature
40.0
-
60.0
°C
Drying Temperature
80.0
-
90.0
°C
@Time 7200 - 14400 sec
Moisture Content
>= 0.010 %
Back Pressure
2.94
-
5.88
MPa
Screw Speed
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
LG Chemical HI855M PMMA, Impact Resistant Grade
LG Chemical AF342 ABS, Flame Retardant
LG Chemical SG175 ABS, Super Surface Gloss
LG Chemical HF380 ABS, Injection Molding
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
PLHCHEM9958 / 239474
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.