  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synthos PS GP 152 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Characteristics: SYNTHOS PS GP 152 is general purpose polystyrene (GPPS) with excellent optical properties, gloss and increased heat resistance. It is a thermoplastic material designed for injection moulding, extrusion, thermoforming and blow extrusion. SYNTHOS PS GP 152 is a colorless plastic. Product has a form of cylindrical granules of diameter 2.5 to 6 mms. Product may contain small amounts of granulate finer than that mentioned above of irregular shapes. Presence of any mechanical impurities in the granulate is not allowed.

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.650 g/cc0.0235 lb/in³apparent
 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption 0.10 %0.10 %Ø 50x3 mm; ISO 62
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/in50x50 mm
Melt Flow 2.5 - 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.5 - 3.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Chemical PropertiesMetricEnglishComments
Styrene Content 0.030 %0.030 %Residual
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 115 MPa16700 psiH 358/30, Ø 50x4 mm; ISO 2039-1
Tensile Strength at Break 45.0 MPa6530 psi5 mm/min; ISO 527-2/1A/5
Elongation at Break 2.0 %2.0 %5 mm/min; ISO 527-2/1A/5
Modulus of Elasticity 3.10 GPa450 ksi1 mm/min; ISO 527-2/1A/1
Flexural Strength 80.0 MPa11600 psi2 mm/min; 80x10x4 mm; ISO 178
Flexural Strain at Break 3.0 %3.0 %2 mm/min; 80x10x4 mm; ISO 178
Charpy Impact Unnotched 1.60 J/cm²7.61 ft-lb/in²80x10x4 mm; ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °F80x10x4 mm; ISO 75-2/Af
Vicat Softening Point  90.0 °C
@Load 5.10 kg
194 °F
@Load 11.2 lb
50 °C/h, 10x10x4 mm; ISO 306/B50
 95.0 °C
@Load 1.02 kg
203 °F
@Load 2.25 lb
50 °C/h, 10x10x4 mm; ISO 306/A50
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 260 °C356 - 500 °FInjection moulding
 200 - 240 °C392 - 464 °FExtrusion
Mold Temperature 10.0 - 60.0 °C50.0 - 140 °FInjection moulding
Dry Time  1.00 hour
@Temperature 70.0 °C
1.00 hour
@Temperature 158 °F
drier with a molecular sieve
 2.00 - 4.00 hour
@Temperature 70.0 °C
2.00 - 4.00 hour
@Temperature 158 °F
hot-air drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSYNTHOS146 / 320427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.