MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synthos PS GP 152 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Characteristics: SYNTHOS PS GP 152 is general purpose polystyrene (GPPS) with excellent optical properties, gloss and increased heat resistance. It is a thermoplastic material designed for injection moulding, extrusion, thermoforming and blow extrusion. SYNTHOS PS GP 152 is a colorless plastic. Product has a form of cylindrical granules of diameter 2.5 to 6 mms. Product may contain small amounts of granulate finer than that mentioned above of irregular shapes. Presence of any mechanical impurities in the granulate is not allowed.

Information provided by Synthos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.650 g/ccapparent
 1.04 g/ccISO 1183
Water Absorption 0.10 %Ø 50x3 mm; ISO 62
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm50x50 mm
Melt Flow 2.5 - 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Chemical PropertiesOriginal ValueComments
Styrene Content 0.030 %Residual
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 115 MPaH 358/30, Ø 50x4 mm; ISO 2039-1
Tensile Strength at Break 45.0 MPa5 mm/min; ISO 527-2/1A/5
Elongation at Break 2.0 %5 mm/min; ISO 527-2/1A/5
Modulus of Elasticity 3.10 GPa1 mm/min; ISO 527-2/1A/1
Flexural Strength 80.0 MPa2 mm/min; 80x10x4 mm; ISO 178
Flexural Strain at Break 3.0 %2 mm/min; 80x10x4 mm; ISO 178
Charpy Impact Unnotched 16.0 kJ/m²80x10x4 mm; ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C80x10x4 mm; ISO 75-2/Af
Vicat Softening Point 90.0 °C
@Load 5.10 kg
50 °C/h, 10x10x4 mm; ISO 306/B50
 95.0 °C
@Load 1.02 kg
50 °C/h, 10x10x4 mm; ISO 306/A50
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 260 °CInjection moulding
 200 - 240 °CExtrusion
Mold Temperature 10.0 - 60.0 °CInjection moulding
Dry Time 1.00 hour
@Temperature 70.0 °C
drier with a molecular sieve
 2.00 - 4.00 hour
@Temperature 70.0 °C
hot-air drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSYNTHOS146 / 320427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.