MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bayshore Vinyl Compounds BVC 6200-65 Vinyl Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: BVC 6200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a smooth semi-gloss finish. Typical applications are window components, weather stripping, tubing, profiles and a variety of injection molded items.

Information Provided by Bayshore Vinyl Compounds Inc., a Mexichem Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65
@Time 10.0 sec
ASTM D2240
Tensile Strength at Break 1632 psiASTM D638
Elongation at Break 391 %ASTM D638
100% Modulus 0.626 ksi
@Strain 100 %
ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -38.0 °CImpact Brittleness; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyether Ester Elastomer
Overview of materials for PVC, Flexible Grade
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound
Colorite Polymers Vinylbond 95-950-65 PVC Compound
Overview of materials for PVC, Extruded

PBAYS005 / 93277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.