MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Yellow Poplar Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Hardwood. Easy to work with hand tools. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Fine/medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Large
Resistance to fungal decay (Heartwood in ground contact): Perishable (Under 5 years), Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Pallet blocks, box boards, turnery. Wood wool

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Populus spp.; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.380 g/ccOven Dry Weight/Unseasoned Volume
 38.0 lb/ft³Unseasoned*
Cell Length 1.90 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1500 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1900 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2400 NSide
Tensile Strength, Ultimate 3.70 MPaPerpendicular to Grain
 155 MPaAxial
 460 psiPerpendicular to Grain*
Modulus of Rupture 0.0700 GPaIn Bending
 5.60 ksiStatic Bending*
Flexural Yield Strength 42.1 MPaBending stress at proportional limit
 3200 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 10.9 - 11.0 GPaIn Bending
 1210 ksiStatic Bending*
Compressive Strength 3.90 MPaPerpendicular to Grain
 37.9 - 38.0 MPaParallel to Grain
 310 psiPerpendicular to Grain*
 2000 psiParallel to Grain*
 2550 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.019µTL, 12% Moisture Content
 0.030µRL, 12% Moisture Content
 0.318µLR, 12% Moisture Content
 0.329µTR, 12% Moisture Content
 0.392µLT, 12% Moisture Content
 0.703µRT, 12% Moisture Content
Machinability 50 %Medium Relative to Other Wood
Shear Strength 8.20 MPaOrientation Unknown
 790 psiParallel to Grain*
Impact 2.6in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 8000psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.480 in-lb/in³Static Bending*
Work to Maximum Load 5.60 in-lb/in³Static Bending*
Toughness 23.8 JTangential
 24.9 JRadial
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.750 BTU-in/hr-ft²-°FOven Dry
 0.900 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.0 %Radial; Green to Zero Moisture
 7.1 %Tangential; Green to Zero Moisture
 12.3 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorGrey, white to pale brown Usual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Balsam Poplar Cottonwood Wood
European Poplar Wood
Tropical Balsa Wood
American Black Walnut Wood
Plywood

PTSAX / 71307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.