MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reliance Industries Reclair Crosslinked R35042
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Crosslinkable R35042 is a polyethylene grade that has increased service temperature and toughness, and improved ESCR over Reclair R35042. Crosslinkable R35042 applications include fuel tanks and chemical tanks.

Information provided by Reliance Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Environmental Stress Crack Resistance >= 400 hour
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17.0 MPaASTM D368
Elongation at Yield 210 %
Flexural Modulus 0.740 GPa
Izod Impact, Notched 240 J/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
Micropol Microlink XL28/FR Black Crosslinkable Polyethylene
LyondellBasell Aquathene® FR409800 Polyethylene Wire and Cable Compound
LyondellBasell Aquathene PM 92949C
LyondellBasell Aquathene CM 04483

PREL021 / 65362

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.