MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Process Stability TOTAL Petrochemicals Polypropylene 3764 features excellent processability and gas fade resistance.

FDA. 3764 complies with all applicable FDA regulations for food contact applications

Recommended Applications. 3764 is recommended for spunbond nonwoven fabric high speed melt spinning applications, and multifilament yarns.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Melt Flow 25 g/10 minASTM D1238, L
 
Mechanical PropertiesOriginal ValueComments
Elongation at Yield 150 %ASTM D3218
Tenacity 2.30 g/denierASTM D3218
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
 
Processing PropertiesOriginal ValueComments
Melt Temperature 204 - 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating
Total PPR 7860 Controlled Rheology Grade Propylene Copolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns and Extrusion Coating
ExxonMobil PP3546G Homopolymer Grade for Ultra-High Melt Flow Rate Nonwoven Applications
ExxonMobil PP3155 Homopolymer Grade for Nonwoven and Fiber Applications
Celanese Celaire™ Acetate Nonwoven

PTOTAL817 / 130542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.