MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Latilon 30D G/10-V0 PC, 10% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled; Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/cc
Linear Mold Shrinkage, Flow 0.0045 - 0.0065 cm/cm
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPa
@Temperature 60.0 °C
 45.0 MPa
@Temperature 23.0 °C
Elongation at Break 28 %
@Temperature 60.0 °C
 35 %
@Temperature 23.0 °C
 >= 100 %
@Temperature 90.0 °C
 >= 100 %
@Temperature 120 °C
Elongation at Yield 2.2 %
@Temperature 120 °C
 2.8 %
@Temperature 90.0 °C
 3.0 %
@Temperature 60.0 °C
 4.0 %
@Temperature 23.0 °C
Tensile Modulus 2200 MPa
@Temperature 120 °C
 2800 MPa
@Temperature 90.0 °C
 2900 MPa
@Temperature 60.0 °C
 3100 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched NB
@Temperature 23.0 °C
 NB
@Temperature -20.0 °C
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -20.0 °C
 7.50 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
Vicat Softening Point 145 °C
@Load 5.00 kg
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
Oxygen Index 34 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
Glow Wire Ignition Temperature 850 °C
@Thickness 1.00 mm
 850 °C
@Thickness 2.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °C
Mold Temperature 100 - 120 °C
Drying Temperature 120 - 130 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kotec Carbotex KGN-10MRA Polycarbonate, Flame Retardant, 10% Glass Fiber Reinforced
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced

PLATH9849 / 177545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.