MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Master Bond UV10TKMed One component UV curable, biocompatible, high viscosity compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond UV10TKMed is a higher viscosity, one part UV system for bonding, sealing and coating that passes USP Class VI testing along with ISO 10993-5 for cytotoxicity. It has good optical clarity, sterling physical properties, a very high glass transition temperature (Tg) that exceeds 140°C and exemplary resistance to repeated sterilization. UV10TKMed cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and, of course, the intensity of the light source. It should be noted that the system can cure in sections up to ¼ inch. However, when bonding, sections of a few thousandths of an inch are more than adequate. Master Bond UV10TKMed is not oxygen inhibited and therefore does not require any special treatment in that regard. It bonds well to glass, composites, surface treated metals and plastics such as polycarbonates and acrylics, among others. It is widely used in medical devices because of its capability of withstanding repeated sterilizations, including radiation, ethylene oxide, chemical sterilants and especially autoclaving. UV10TKMed is not only effective for bonding applications; it can also be used as a coating or sealant. The system does not contain any solvents or diluents and none are released during cure. UV10TKMed combines low shrinkage with dimensional stability. Its service temperature range is -60°F to +450°F. UV10TKMed is a superlative electrical insulator. It is most effectively used in medical device manufacturing where rapid fixture times, fast curing and audacious temperature resistance are needed. UV10TKMed can be employed in a wide variety of application scenarios involving both disposable and reusable medical device manufacturing. The uniqueness of the product is based on its high temperature resistance and its ability to withstand repeated sterilizations along with a rapid UV curing mechanism.

Product Advantages:

  • Convenient mix ratio; 100:30 by weight
  • Low viscosity, easy to apply; very One component system; no mixing needed; ready to use as supplied
  • Very fine electrical insulator
  • High bond strength; excellent adhesion to surface treated metals, glass and many plastics
  • Enhanced ability to withstand repeated chemical and heat sterilizations

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 35000 - 45000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 65
Tensile Strength at Break >= 8000 psi
@Temperature 23.9 °C
Tensile Modulus >= 350000 psi
@Temperature 23.9 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.8
@Frequency 60 Hz,
Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 - 50.0 µm/m-°C
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -60.0 °F
Glass Transition Temp, Tg >= 140 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.557
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 23.9 °C
in original unopened containers with no exposure to light
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal
MarkeTech Rutile (TiO2) Fiber Optic Crystal

PMASTB328 / 149575

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.