MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Universal Wire Works 309 Stainless Steel Electrode
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Universal 309 electrodes are used for the welding of heat resisting type 309 stainless steel. Deposits retain strength and oxidation resistance up to 2000 degrees F. Typical applications include furnace parts, kiln linings, and heat treat baskets. Alloy 309 is excellent for welding AISI types 405, 410, 430, 442, and 446 when preheat and postweld heat treatment is not practical. Alloy 309 is also used for welding the clad side of stainless clad steels and for joining mild or carbon steels to stainless steel.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS E309-15,16
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 87000 psi
Elongation at Break 40 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.10 %
Chromium, Cr 23.4 %
Iron, Fe 61 %As Remainder
Manganese, Mn 1.8 %
Nickel, Ni 13.1 %
Silicon, Si 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
309 Stainless Steel
301 Stainless Steel
Special Metals INCOLOY® alloy 832 Stainless Steel
Universal Wire Works 309L Stainless Steel Electrode
310 Stainless Steel, annealed sheet

NUWW004 / 19588

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.