MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec ZN 40 Zirconia, ZrO2-MgO
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like thermal expansion attributes, make this material an ideal partner for bearing composites working at elevated temperatures.

Key Words: Zirconium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.74 g/ccDIN EN 623-2
Water Absorption 0.00 %Open Porosity; DIN EN 623-2
Permeability 0.00%, Gas
Weibull Modulus 25DINV ENV 843-5
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1240HV1; DINV ENV 843-4
Tensile Strength at Break 500 MPaACMA Test #4 / DIN EN 843-1
Tensile Modulus 210 GPaYoung's; DINV ENV 843-2
Flexural Strength 500 MPaDIN EN 843-1
Compressive Strength 1600 MPaDIN 51067T1
Poissons Ratio 0.30DINV ENV 843-2
Fracture Toughness 8.10 MPa-m½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 80.8 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 500000 ohm-cm
@Temperature 400 °C
IEC 672-1
 5.00e+13 ohm-cm
@Temperature 20.0 °C
IEC 672-1
Dielectric Constant 27
@Frequency 1e+6 Hz
IEC 672-1
Dielectric Strength 19.0 kV/mmIEC 672-1
Dielectric Loss Index 0.020
@Frequency 9.00e+9 Hz
IEC 672-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.2 µm/m-°C
@Temperature 20.0 - 400 °C
DIN EN 821-1
 11.0 µm/m-°C
@Temperature 20.0 - 1000 °C
DIN EN 821-1
Specific Heat Capacity 0.400 J/g-°CDINV ENV 821-3
Thermal Conductivity 3.00 W/m-KDIN EN 821-2
Maximum Service Temperature, Air 850 °C
Maximum Service Temperature, Inert 850 °C
 
Descriptive Properties
Ra = Arithmetic Mean Roughness Value (µm)<0.06
Thermal Shock Resistance R1 (K)163calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec 848 Zirconia, ZrO2•MgO
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
CeramTec MZ 429 Zirconia, ZrO2-Y2O3
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2

CCERA909 / 107509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.