MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Novec™ 7100DL Engineered Fluid
Categories: Fluid

Material Notes: A higher purity version of 3M™ Novec™ 7100, 3M™ Novec™ 7100DL is tightly-controlled for ions, metals and non-volatile residue. It is used in precision cleaning and deposition applications when high-purity materials are needed.

Features and Benefits:

  • Non-flammable
  • Non-conductive
  • Compatible with plastics
  • Low toxicity
  • Low Global Warming Potential (GWP)
  • Zero ozone depletion potential
  • VOC-exempt solvent (US EPA)
  • Low surface tension penetrates tight spaces for improved cleaning
  • High purity

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccLiquid
Solubility in Water <= 0.0012 %
Solubility 95 ppm
Viscosity 0.58 cP
Molecular Weight 250 g/mol
Vapor Pressure 0.267 bar
Surface Tension 13.6 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 113 J/g
Specific Heat Capacity 1.17 J/g-°C
Boiling Point 61.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Novec™ 774 Engineered Fluid
3M Novec™ 71DA Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid

PMM33103 / 167850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.