MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. This balance of engineering properties in combination with excellent processability make it ideal in applications replacing metal, resulting in an overall cost and weight savings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183
Water Absorption 1.1 %24 hour; ISO Test
 6.4 %ISO 62
Moisture Absorption at Equilibrium 1.8 %23°C/50% R.H.; ISO 62
Relative Viscosity 2.6 cPISO Test; 96 % SAV
Viscosity Measurement 50Formic Acid
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM Test
Tensile Strength at Break 180 MPa0.2 in/min; ASTM Test
 70.0 MPa
@Temperature 120 °C
ASTM Test
 70.0 MPa
@Temperature 120 °C
ISO Data
 90.0 MPa
@Temperature 80.0 °C
ISO Data
 90.0 MPa
@Temperature 80.0 °C
ASTM Test
 230 MPa
@Temperature -40.0 °C
ASTM Test
 230 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Ultimate 170 MPa5mm/min; ISO 527
Elongation at Break 3.0 %5mm/min; ISO 527
 3.5 %0.2 in/min; ASTM Test
Tensile Modulus 10200 MPa1mm/min; ISO 527
 4010 MPa
@Temperature 120 °C
ISO Data
 4820 MPa
@Temperature 80.0 °C
ISO Data
 10300 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 245 MPaISO Data
 280 MPaASTM Test
Flexural Modulus 8500 MPaISO Data
 8990 MPaASTM Test
Izod Impact, Notched 1.10 J/cm
@Thickness 3.17 mm
ASTM Test
Charpy Impact Unnotched 6.50 J/cm²ISO 179
Charpy Impact, Notched 1.00 J/cm²ISO 179
 1.00 J/cm²
@Temperature -30.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75
 218 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75
 208 °CASTM Test
Flammability, UL94 HB
@Thickness 0.710 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 °CInjection molding
Mold Temperature 95.0 °CInjection molding
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)

PBASF9163 / 84927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.