MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach P-20 Modified Plastic Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes: Description: P-20 Modified is an improved pre-hardened mold steel that has been specially designed for large plastic molds; The material is forged on a 5000 ton press assuring maximum deformation during the forging process; Hardness loss in large cross sections is minimal

Characteristics: Good polishability; Good compressive strength; Minimum hardness loss in large cross section

Applications: Injection molds, Compression molds, Mold frame, Forming tools and Die holder

Stress Relieving (Heat Treatment): 850°F-900°F hold 1 hr/in; Cooling: Air cool; Note: Large cross sections require accurate control of temperatures and times

Information provided by Schmolz + Bickenbach

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.284 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 33
@Treatment Temp. 621 °C,
Time 7200 sec
 35
@Treatment Temp. 593 °C,
Time 7200 sec
 40
@Treatment Temp. 566 °C,
Time 7200 sec
 43
@Treatment Temp. 538 °C,
Time 7200 sec
 47
@Treatment Temp. 482 °C,
Time 7200 sec
 50
@Treatment Temp. 427 °C,
Time 7200 sec
 51
@Treatment Temp. 371 °C,
Time 7200 sec
Tensile Strength 150 ksi
@Temperature -5.56 °C
Hardened and tempered to 34 HRC
Tensile Strength, Yield 130 ksi
@Temperature 22.0 °C
Hardened and tempered to 34 HRC
Elongation at Yield 15 %
@Temperature 22.0 °C
Hardened and tempered to 34 HRC
Reduction of Area 35 %
@Temperature 22.0 °C
Hardened and tempered to 34 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.80 µin/in-°F
@Temperature 21.1 - 93.3 °C
 7.00 µin/in-°F
@Temperature 21.1 - 204 °C
 7.10 µin/in-°F
@Temperature 21.1 - 302 °C
Thermal Conductivity 202 BTU-in/hr-ft²-°F
@Temperature 21.1 °C
 209 BTU-in/hr-ft²-°F
@Temperature 204 °C
 216 BTU-in/hr-ft²-°F
@Temperature 427 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.34 %
Chromium, Cr 1.75 %
Iron, Fe 96.31 %
Manganese, Mn 0.80 %
Molybdenum, Mo 0.40 %
Silicon, Si 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Schmolz + Bickenbach P-20 High Hard Plastic Mold Steel
EDRO #3 Prehardened Mold Quality P20 Alloy Steel
AISI Type P20 Mold Steel (UNS T51620)
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections

NSCHMO004 / 125877

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.