MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7178-T76; 7178-T7651
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes: Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97178; Aluminium 7178-T76; Aluminium 7178-T7651; AA7178-T76; AA7178-T7651; Al7178-T76
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 152152500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 193193Converted from Brinell Hardness Value
Hardness, Rockwell A 53.953.9Converted from Brinell Hardness Value
Hardness, Rockwell B 8888Converted from Brinell Hardness Value
Hardness, Vickers 177177Converted from Brinell Hardness Value
Tensile Strength, Ultimate 572 MPa83000 psiAA; Typical
 45.0 MPa
@Temperature 371 °C
6530 psi
@Temperature 700 °F
 59.0 MPa
@Temperature 316 °C
8560 psi
@Temperature 601 °F
 76.0 MPa
@Temperature 260 °C
11000 psi
@Temperature 500 °F
 105 MPa
@Temperature 204 °C
15200 psi
@Temperature 399 °F
 215 MPa
@Temperature 149 °C
31200 psi
@Temperature 300 °F
 475 MPa
@Temperature 100 °C
68900 psi
@Temperature 212 °F
 570 MPa
@Temperature 24.0 °C
82700 psi
@Temperature 75.2 °F
 605 MPa
@Temperature -28.0 °C
87700 psi
@Temperature -18.4 °F
 625 MPa
@Temperature -80.0 °C
90600 psi
@Temperature -112 °F
 730 MPa
@Temperature -196 °C
106000 psi
@Temperature -321 °F
Tensile Strength, Yield 503 MPa73000 psiAA; Typical
 38.0 MPa
@Strain 0.2 %,
Temperature 271 °C
5510 psi
@Strain 0.2 %,
Temperature 520 °F
 48.0 MPa
@Strain 0.2 %,
Temperature 316 °C
6960 psi
@Strain 0.2 %,
Temperature 601 °F
 62.0 MPa
@Strain 0.2 %,
Temperature 260 °C
8990 psi
@Strain 0.2 %,
Temperature 500 °F
 83.0 MPa
@Strain 0.2 %,
Temperature 204 °C
12000 psi
@Strain 0.2 %,
Temperature 399 °F
 185 MPa
@Strain 0.2 %,
Temperature 149 °C
26800 psi
@Strain 0.2 %,
Temperature 300 °F
 440 MPa
@Strain 0.2 %,
Temperature 100 °C
63800 psi
@Strain 0.2 %,
Temperature 212 °F
 505 MPa
@Strain 0.2 %,
Temperature 24.0 °C
73200 psi
@Strain 0.2 %,
Temperature 75.2 °F
 525 MPa
@Strain 0.2 %,
Temperature -28.0 °C
76100 psi
@Strain 0.2 %,
Temperature -18.4 °F
 540 MPa
@Strain 0.2 %,
Temperature -80.0 °C
78300 psi
@Strain 0.2 %,
Temperature -112 °F
 615 MPa
@Strain 0.2 %,
Temperature -196 °C
89200 psi
@Strain 0.2 %,
Temperature -321 °F
Elongation at Break  10 %
@Temperature -196 °C
10 %
@Temperature -321 °F
 10 %
@Temperature -80.0 °C
10 %
@Temperature -112 °F
 10 %
@Temperature -28.0 °C
10 %
@Temperature -18.4 °F
 11 %
@Temperature 24.0 °C
11 %
@Temperature 75.2 °F
 17 %
@Temperature 100 °C
17 %
@Temperature 212 °F
 40 %
@Temperature 149 °C
40 %
@Temperature 300 °F
 70 %
@Temperature 204 °C
70 %
@Temperature 399 °F
 76 %
@Temperature 260 °C
76 %
@Temperature 500 °F
 80 %
@Temperature 316 °C
80 %
@Temperature 601 °F
 80 %
@Temperature 371 °C
80 %
@Temperature 700 °F
 11 %
@Diameter 12.7 mm
11 %
@Diameter 0.500 in
AA; Typical
Modulus of Elasticity 71.0 GPa10300 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
 73.0 GPa10600 ksi
Compressive Yield Strength 460 MPa66700 psi0.1% Permanent Set
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Fatigue Strength 160 MPa
@# of Cycles 5.00e+8
23200 psi
@# of Cycles 5.00e+8
Shear Modulus 27.0 GPa3920 ksiEstimated from similar Al alloys.
Shear Strength 340 MPa49300 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000500 ohm-cm0.00000500 ohm-cmEstimated from other heat treatments.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.1 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 24.4 µm/m-°C
@Temperature 20.0 - 200 °C
13.6 µin/in-°F
@Temperature 68.0 - 392 °F
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
14.1 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.856 J/g-°C0.205 BTU/lb-°F
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°FEstimated from other heat treatments.
Melting Point 477 - 629.4 °C890 - 1165 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Homogenization may raise eutectic melting temperature 20-40°F but usually does not eliminate it.
Solidus 477 °C890 °FAA; Typical
Liquidus 629.4 °C1165 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 468 °C875 °F
Aging Temperature 121 °C250 °Ffor 24 hr
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 85.3 - 89.5 %85.3 - 89.5 %As remainder
Chromium, Cr 0.18 - 0.28 %0.18 - 0.28 %
Copper, Cu 1.6 - 2.4 %1.6 - 2.4 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 2.4 - 3.1 %2.4 - 3.1 %
Manganese, Mn <= 0.30 %<= 0.30 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.40 %<= 0.40 %
Titanium, Ti <= 0.20 %<= 0.20 %
Zinc, Zn 6.3 - 7.3 %6.3 - 7.3 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7178-T6; 7178-T651
Aluminum 7075-T6; 7075-T651
Aluminum 7178-T6; 7178-T651 (Included Creep/Rupture Data)
Aluminum 7475-T7651
Aluminum 7175-T736; 7175-T7365x

MA7178T76 / 9621

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.