MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic

Material Notes: AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, very low moisture absorption, is thermoformable and ductile. AIREX® R82 is a core material for use in structural lightweight applications that demand high fire resistance, radar transparency or operation in extremely hot or cold environments.

Characteristics

  • Fulfils most stringent fire requirements
  • Operating temperature from -194°C to +160°C (-317° F to +320 °F)
  • Remains ductile at cryogenic temperatures
  • Excellent dielectric properties (radar transparent outstanding)
  • Very low moisture absorption
  • Good fatigue resistance
  • High impact resistance (non-brittle failure mode)
  • Thermoformable
  • Good sound and thermal insulation
Applications
  • Aircraft and Aerospace: Interiors, cockpit doors, cryogenic tanks, insulating panels, radomes, helicopter rotor blades, general aviation (fuselage and wing)
  • Road and Rail: Front-ends, side skirts, roof panels, interiors
  • Marine: Fast-ferries, fire resistant interiors, radomes
  • Defense: Naval superstructures, antennas, combat communication systems
  • Industrial: High-temperature tooling, radomes, x-ray tables
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0800 g/ccaverage; ISO 845
 0.0720 - 0.0950 g/cctypical range; ISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 1.70 MPain the plane; ISO 527 1-2
 2.00 MPaaverage; in the plane; ISO 527 1-2
Elongation at Break >= 15 %shear; ISO 1922
 23 %average; shear; ISO 1922
Tensile Modulus >= 50.0 MPain the plane; ISO 527 1-2
 54.0 MPaaverage; in the plane; ISO 527 1-2
Compressive Strength >= 0.900 MPaperpendicular to plane; ISO 844
 1.10 MPaaverage; perpendicular to plane; ISO 844
Compressive Modulus >= 56.0 MPaperpendicular to plane; DIN 53421
 62.0 MPaaverage; perpendicular to plane; DIN 53421
Shear Modulus >= 0.0200 GPaASTM C393
 0.0230 GPaaverage; ASTM C393
Shear Strength >= 0.900 MPaISO 1922
 1.10 MPaaverage; ISO 1922
Charpy Impact, Notched 1.30 kJ/m²DIN 53453
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0370 W/m-KISO 8301
 
Descriptive Properties
Coloroff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam

PZ3AC026 / 108515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.