MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according to EN 1852-1/A1 and is a PP-HM (polypropylene high modulus) material.

BorECO BA222E is recommended for solid wall non-pressure piping especially in underground drainage and sewerage and soil and waste applications.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 g/ccISO 1183
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4786 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 8.0 %At 50 mm/min; ISO 527-2
Flexural Modulus 1.90 GPaAt 2 mm/min; ISO 178
Charpy Impact, Notched 5.00 J/cm²ISO 179/1eA
 0.400 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 200 - 220 °C
Die Temperature 410 - 428 °F
Melt Temperature 210 - 230 °C
Head Temperature 210 - 220 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Borealis BC142MO Polypropylene Copolymer
Borealis BC612WG Polypropylene Copolymer

PBOREA012 / 27319

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.