MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® LR 6262 A/B US Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 6262 A/B US is a two-component liquid silicone rubber system that cures rapidly upon heating to a tough silicone rubber. It has been formulated primarily as a heat resistant adhesive coating to be used in fabric lamination or between other substrates.

Special features:

  • 100% solids - no solvent
  • Made in the U.S.A.
  • Good adhesion to various substrates
  • Excellent mechanical properties

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D412
Viscosity 200000 cPASTM D2240
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40 - 50ASTM D2240
Tensile Strength 1000 psiASTM D412
Elongation at Break 350 %ASTM D412
Tear Strength 160 plidie B; ASTM D624
 
Processing PropertiesOriginal ValueComments
Mold Temperature 166 °C
@Thickness 1.91 mm
Compression molded, cold mold/heated press, 5 minutes press time
Cure Time 1.00 - 6.00 min
@Temperature 172 - 200 °C
oven cure
Pot Life 1440 min
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® R 427/30 High Strength Silicone Base
Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade
Wacker ELASTOSIL® R plus 4070/20 Self-Adhesive TV Silicone Rubber
Wacker ELASTOSIL® LR 3066/30 A/B Liquid Silicone Rubber with Low Frictional Coefficient
Dow Silastic® 9252/150P A&B KIT

PWACK9901 / 197500

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.